OXIDATION OF PM ALLOY Al-10Ti DURING SLIDING WEAR
Wu Nianqiang; Wang Guangxin; Li Zhizhang

Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027

Abstract:Sliding wear behaviors of PM alloy Al 10Ti have been investigated. The compositions and structures of worn surface layer and wear debris have been studied using XPS and X ray diffraction. The results show that iron transfers from the steel counterface to the surface of Al Ti alloy sample. And Fe2O3 is formed during sliding wear process. The dark worn surface layer formed in sliding wear is determined to be an oxide layer consisting of Al2O3 and Fe2O3, which is rich in oxygen and aluminum, but depleted of titanium. The oxide layer can reduce wear of aluminum alloy.

 

Key words: oxidation sliding wear Al Ti alloy

ISSN 1672-7029
CN 43-1423/U

主管:中华人民共和国教育部 主办:中南大学 中国铁道学会 承办:中南大学
湘ICP备09001153号 版权所有:《铁道科学与工程学报》编辑部
------------------------------------------------------------------------------------------
地 址:湖南省长沙市韶山南路22号 邮编:410075
电 话:0731-82655133,82656174   传真:0731-82655133   电子邮箱:jrse@mail.csu.edu.cn