Preparation and microwave dielectric properties of Csf/Si3N4 composites
WANG Xiao-yan(王晓艳), LUO Fa(罗  发), LI Peng(李  鹏), SU Xiao-lei(苏晓磊),
ZHU Dong-mei(朱冬梅), ZHOU Wan-cheng(周万城)

State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072, China

Abstract:The Csf/Si3N4 composites were prepared by hot-press sintering method using α-Si3N4 power, short carbon fibers and La2O3-Y2O3 sintering additives. The mechanical and microwave dielectric properties of Csf/Si3N4 composites were studied and discussed. The results show that the addition of the short carbon fibers can not destroy the relative density of the sintered samples, but it deteriorates the flexural strength of the sintered samples, so the flexural strength of the silicon nitride matrix is the highest among the samples. The real part (ε′) and the imaginary part (ε″) of the permittivity of Csf/Si3N4 composites greatly increase with increasing volume fraction of the short carbon fibers, achieve the maximum 73.1 and 101.5, respectively. A strong frequency dependence of the imaginary part (ε″) of the permittivity is observed.

 

Key words: Csf/Si3N4; composites; short carbon fibers; mechanical property; dielectric properties

ISSN 1672-7029
CN 43-1423/U

主管:中华人民共和国教育部 主办:中南大学 中国铁道学会 承办:中南大学
湘ICP备09001153号 版权所有:《铁道科学与工程学报》编辑部
------------------------------------------------------------------------------------------
地 址:湖南省长沙市韶山南路22号 邮编:410075
电 话:0731-82655133,82656174   传真:0731-82655133   电子邮箱:jrse@mail.csu.edu.cn